Has any work been done on a gel-coat like material that can be used with graphite epoxy pre-preg? That would be applied during lay-up and would take the place of paint.
 
Replies continue below

Recommended for you

gab4055 (Aerospace)
There are several forms of in mold coating that can be used in place of gel-coat. Were you looking for a film material or a sprayable in mold coating?
An example of a sprayable in mold coating would be Futura polyurethane gel coat. by ITW Futura coatings Inc.,
B.E.
 
Either one would work. A film would be perfered
 