Can anybody explain me the effect of CaCO3 concentration on the UV stabilizer?. I´m Working with PP extrusion process to produce flat tapes for textile use.
 
Replies continue below

Recommended for you

Hi
Certainly addition of CaCO3 helps increase in UV stability of PP Tapes to some extent but the main advantage is the antifibrilation properties.