anyone know of any work published on this realcion of between 6.2 and 6.3 in the table related to the reduction in effort of tension or something similar
AWS D1.1 secc. Table 6.2 and 6.3
 
urgent, Spanish, in Deutsch better.. English not problem
 
You realize that one table is for static (non-cyclical) nontubular structures and the other is for cylic nontubular structures, correct? That is why the acceptance criteria is different. I'm not sure if this helps you or not, but that is the relation between the two tables. I'm unaware of any published work on the subject. You might want to contact someone at AWS directly.
 
ok, yes I mean 6.2.

yes i did last year contac AWS committee, but they said, only to committe group is permited
 
I m Just looking for a document Publicated on the web or in a manual that says something about the relationship between UtdB and tensile

I hope someone can help me.
 
Check with Krautkramer-Bransen. They have published documents on UT attenuation and tensile strength of materials.

For steel, it is generally calibrated at each use by a certified calibration block.
 
Thank you,
I did not think in Krautkramer,, I will do. thank you
 
I someone knows somethingh else teel me please
 