Guest102023
Materials
The weld overlay cladding is 4 layers (~½") of Inconel on a carbon steel substrate. In metallographic cross sections we are seeing partially mixed zones with features up to ¼ inch in dimension, greater than our acceptance criterion. Everything is vertically situated within 0.05" of the fusion line. There is no actual discontinuity.
My question is for UT experts: Since the two materials have different acoustical properties, could these metallurgical effects show up as discontinuities by UT exam?
"If you don't have time to do the job right the first time, when are you going to find time to repair it?"
My question is for UT experts: Since the two materials have different acoustical properties, could these metallurgical effects show up as discontinuities by UT exam?