ASME SA-788 S20 lists two recommended UT acceptance levels (BR and DA) for forgings. Can someone help me find what these designations mean and where they come from?
 
Replies continue below

Recommended for you

I just reviewed SA 788. The above terms are defined;

BR - back reflection method for striaght beam testing

DA - Distance amplitude

The above UT methods are discussed in SA 388.
 