Dec 11, 2012 #1 metalonis Mechanical Joined Feb 28, 2002 Messages 183 Location US ASME SA-788 S20 lists two recommended UT acceptance levels (BR and DA) for forgings. Can someone help me find what these designations mean and where they come from?
ASME SA-788 S20 lists two recommended UT acceptance levels (BR and DA) for forgings. Can someone help me find what these designations mean and where they come from?
Dec 11, 2012 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US I just reviewed SA 788. The above terms are defined; BR - back reflection method for striaght beam testing DA - Distance amplitude The above UT methods are discussed in SA 388. Upvote 0 Downvote
I just reviewed SA 788. The above terms are defined; BR - back reflection method for striaght beam testing DA - Distance amplitude The above UT methods are discussed in SA 388.
Dec 11, 2012 Thread starter #3 metalonis Mechanical Joined Feb 28, 2002 Messages 183 Location US Thanks ME. Upvote 0 Downvote