WE are manufacturing a Cupro-Nickel Heat exchanger according to ASME VIII div. I -U stamped- and we have some problem to find S.O. flanges because the only flanges that we are able to find is made of SB 151-C70600, but this material is not permitted by the ASME VIII div. I, even if is included in the ASME II part B. Can someone suggest me a way to exit from this problem?, using the SB151 and not the SB171?
Thank You