SA358 is a material grade included in ASME IIA as an ASME recognised material.
The specification is for Electron Fusion Welded Pipe with the addition of filler metal.
However in ASME VIII section UG-8 sub note 3, it states that pipe or tube welded with the addition of filler metal may not be used for code construction.
Therefore it what circumstances would SA358 pipe be acceptable for use in vessel construction.
Must it only be supplied with a partial data report (manufactured by a ASME certified shop) ?
Any feedback would be appreciated.
Thanks in advance.
lee
The specification is for Electron Fusion Welded Pipe with the addition of filler metal.
However in ASME VIII section UG-8 sub note 3, it states that pipe or tube welded with the addition of filler metal may not be used for code construction.
Therefore it what circumstances would SA358 pipe be acceptable for use in vessel construction.
Must it only be supplied with a partial data report (manufactured by a ASME certified shop) ?
Any feedback would be appreciated.