Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations Ron247 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Using localized heat to fuse UHMWPE and others

Status
Not open for further replies.

TurboLS

Materials
Jan 2, 2007
38
Hey guys. I am a newcomer to this forum. I am trying to get fully cured or even B-stage ultra high molecular weight polyethylene to fuse to itself with the use of localized heat. I'm just wondering if there is a resource out there that goes over different thermal profiles used in post-process joining. I read over a few of the threads on plastic welding and other adhesive methods, but I haven't found anything definitive.
 
Replies continue below

Recommended for you

thanks again for the info, guys. i'll run some tests when i have a chance.
 