Oct 21, 2014 #1 eadkins73 Mechanical Joined Oct 21, 2014 Messages 10 Location US Has anyone ever heard of using epoxy to attach repads on an ASME Section VIII, Div 1 pressure vessel?
Has anyone ever heard of using epoxy to attach repads on an ASME Section VIII, Div 1 pressure vessel?
Oct 21, 2014 #2 SnTMan Mechanical Joined Jan 22, 2005 Messages 6,858 Location US Metallic vessel? No. Part UIG vessel? Possibly, not familiar enough with it to say. Regards, Mike Upvote 0 Downvote
Oct 21, 2014 #3 weldstan Materials Joined Jun 24, 2011 Messages 2,806 Location US No. Upvote 0 Downvote
Oct 21, 2014 Thread starter #4 eadkins73 Mechanical Joined Oct 21, 2014 Messages 10 Location US Thanks guys. Yes it's a carbon steel vessel. Sorry should have mentioned that. I already told them no but just wanted my ducks in a row in case they asked why. Upvote 0 Downvote
Thanks guys. Yes it's a carbon steel vessel. Sorry should have mentioned that. I already told them no but just wanted my ducks in a row in case they asked why.
Oct 21, 2014 #5 SnTMan Mechanical Joined Jan 22, 2005 Messages 6,858 Location US eadkins73, so you're gonna answer that "weldstan & SnTMan said they never heard of it"? Regards, Mike Upvote 0 Downvote
eadkins73, so you're gonna answer that "weldstan & SnTMan said they never heard of it"? Regards, Mike
Oct 21, 2014 #6 GenB Mechanical Joined Oct 24, 2003 Messages 1,362 Location US Pls, I also say no I need er heard of it... And I never will Upvote 0 Downvote
Oct 22, 2014 Thread starter #7 eadkins73 Mechanical Joined Oct 21, 2014 Messages 10 Location US Will do Mike. LOL Upvote 0 Downvote