May B7 threaded rod be used as cut to length ASTM A 193 stud material?
 
Replies continue below

Recommended for you

Well, what are the material spec's for strength for B7 and for ASTM A 193?

(Let's assume the two threaded rods are cut to the same dimensions. )
 
NDT3RICH, ideally you'd want to transfer markings to the cut end(s) if for Code use.

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
Yes. We do this all the time. Engrave the end with the grade for future reference.
 