Aug 27, 2015 #1 NDT3RICH Petroleum Joined Aug 19, 2015 Messages 12 Location US May B7 threaded rod be used as cut to length ASTM A 193 stud material?
Aug 27, 2015 #2 racookpe1978 Nuclear Joined Feb 1, 2007 Messages 5,995 Location US Well, what are the material spec's for strength for B7 and for ASTM A 193? (Let's assume the two threaded rods are cut to the same dimensions. ) Upvote 0 Downvote
Well, what are the material spec's for strength for B7 and for ASTM A 193? (Let's assume the two threaded rods are cut to the same dimensions. )
Aug 27, 2015 #3 SnTMan Mechanical Joined Jan 22, 2005 Messages 6,862 Location US NDT3RICH, ideally you'd want to transfer markings to the cut end(s) if for Code use. Regards, Mike The problem with sloppy work is that the supply FAR EXCEEDS the demand Upvote 0 Downvote
NDT3RICH, ideally you'd want to transfer markings to the cut end(s) if for Code use. Regards, Mike The problem with sloppy work is that the supply FAR EXCEEDS the demand
Aug 27, 2015 #4 moltenmetal Chemical Joined Jun 5, 2003 Messages 5,504 Location CA Yes. We do this all the time. Engrave the end with the grade for future reference. Upvote 0 Downvote