Is the use of intumescent (fire resistant) paint an acceptable method of reducing the heat input into a vessel or tank from an external pool fire?
If so, how is the heat input calculated?
I know this type of paint has been used on steel structures, but we are being asked to use it on pressure vessels to reduce the heat input. I have doubts if this is acceptable, but would like to hear opinions from others.
Thank you.
 
Replies continue below

Recommended for you

I've never seen credit given for intumescent paint on a pressure vessel. What's the dry film thickness and insulation value? Will it survive the extreme thermal stress seen during a pool fire and then fire water hits it? Sounds like a stretch to me, but then I haven't seen everything, yet.

Good luck,
Latexman
 
Who is asking you to use this ? and based on what requirements ?
It depends if they are looking at all the factors in your equation, as Latexman noted.
Nullfire is a well known supplier of these products Ive never seen a pressure vessel painted for fire protection, more often than not these are protected with flexible fire protection Ciao,
Itascot
 