I am reviewing a design of PV that requires u stamping. Does the code allows use of S355JR for non pressure parts (structural)? S355JR is not listed in ASME II Pt D.Pls help with clarification.
Thanks.
 
Replies continue below

Recommended for you

creator, most likely it is permitted. See UG-4(b), UW-5(b).

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 