Hello
Can you help at all with this issue - I am having unexpected issues with spherical bearings premature wear/damage and locking up/becoming very stiff after very little use
The application is automotive suspension – bearing is a 15mm ID spherical PTFE lined plain spherical (rose joint)
The bearings run in a suspension joint sealed by o-rings – movement is about 20 degrees of rotation around the axis of the fixing bolt
Suspension was rough and sticking / becoming stiff - when removed this is what we found - bearing is very rough to move / locks up in your hand
We are seeing the following damage only after 250miles light use – see photos - the marks are in line with the edges of the outer race - just inside the race so cannot be seen from the outside until the ball is rotated a little
Nothing else in the joint looked out of place or damaged in any way - No obvious contamination was present on disassemble - joint was free from dirt, water, grit etc
the car has 16 of these joints in total 2 per wishbone - its very light (750kg) and has had only light road use, dry conditions, since fitting the joints.
Other users with the same setup seem to have several years use without maintenance or issue !
note in the picture there appears to be two distinct forms of marking on the bearing ball
1, wear through the polished outer surface of the hardened inner ball - this you can feel as a ridge with your finger nail 2, dark brown/black deposits in the center of the bearing surface ( between the other wear marks) - these are smooth and appear to be deposits on top of the ball.
Is this a known issue you have come across before?
since other users have no issues at all - even after extensive track use - could this be a manufacturing issue
if so what could have gone wrong ?
I would be very grateful if you could shed any light on this
Much appreciated
Can you help at all with this issue - I am having unexpected issues with spherical bearings premature wear/damage and locking up/becoming very stiff after very little use
The application is automotive suspension – bearing is a 15mm ID spherical PTFE lined plain spherical (rose joint)
The bearings run in a suspension joint sealed by o-rings – movement is about 20 degrees of rotation around the axis of the fixing bolt
Suspension was rough and sticking / becoming stiff - when removed this is what we found - bearing is very rough to move / locks up in your hand
We are seeing the following damage only after 250miles light use – see photos - the marks are in line with the edges of the outer race - just inside the race so cannot be seen from the outside until the ball is rotated a little
Nothing else in the joint looked out of place or damaged in any way - No obvious contamination was present on disassemble - joint was free from dirt, water, grit etc
the car has 16 of these joints in total 2 per wishbone - its very light (750kg) and has had only light road use, dry conditions, since fitting the joints.
Other users with the same setup seem to have several years use without maintenance or issue !
note in the picture there appears to be two distinct forms of marking on the bearing ball
1, wear through the polished outer surface of the hardened inner ball - this you can feel as a ridge with your finger nail 2, dark brown/black deposits in the center of the bearing surface ( between the other wear marks) - these are smooth and appear to be deposits on top of the ball.
Is this a known issue you have come across before?
since other users have no issues at all - even after extensive track use - could this be a manufacturing issue
if so what could have gone wrong ?
I would be very grateful if you could shed any light on this