I have to qualify a welding procedure for Duplex material (UNS 32205). Which welding wire should I use for welding, and what precautions are to be taken during welding
Merzi,
There can be an expensive learning curve with Duplex, but there are some excellent reference publications available to help you get a good start. Avesta has one which I think is available online at
and the International Molybdenum Association has an even better reference entitled ' Practical Guidelines for the Fabrication of Duplex Stainless Steels'. I believe their website is
Does anyone have extensive experience qualifying WPSs using 2205 to NAVSEA Tech Pub 248 para 4.7.5(f)? Specifically I'm interested in the requirement (if any) to MAINTAIN interpass temperature (vs. ensuring that WPS interpass max is not exceeded).
I would contact Avesta Welding in Orchard Park, NY and see if they can offer assistance specific to your NAVSEA requirements. They make E2209 fillers and their former parent company helped develop the base metal.