How hard is this metal?
the chemistry you give is funny, I would like to say PH13-8Mo, but the Cr and Mn are high, while the Ni and Mo are low...
As mcguire explained to me a few years ago chem. analysis of SS is not quite as easy as carbon steels... Is this an arc&spark (OE spectro) analysis? You might want to try a few burns to see if the values for the elements move around much.
nick