Big1995,
In order to answer your question I would need more information on how you are installing the rivet.
Are you squeeze riveting, using a pneumatic rivet hammer,
or an electromagnetic hammer?
7050 rivets tend to get micro cracks in the formed head if they are formed slowly.
B.E.