Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

uniaxial strain limit - Table 5.7 ASME.BPVC.VIII.2 Chapter 5 1

Status
Not open for further replies.

tigny

Structural
Joined
Mar 12, 2001
Messages
110
Location
FR
hi,

regarding 5.3.3 Protection against local failure, Elastic-plastic analysis - Local Strain Limit,
there are reference parameters εLu, m2 and αsl to be selected in Table 5.7 depending on materials.

Table 5.7 lists Ferritic steel; Stainless steel and Nickel based Alloys; Duplex stainless steel; Precipitation hardenable nickel base alloys and other non ferrous materials.

[ul]
[li]What if the component is made of carbon steel?[/li]
[li]What values of εLu, m2 (formulaes) and αsl should be used for carbon steel?[/li]
[/ul]

best regards
 
Carbon steel is a ferritic steel.
 
Dear TGS4
TGS4 said:
Carbon steel is a ferritic steel.

Thank you for your answer, I'm sorry I didn't react before.

I was having a confusion between Carbon steels (therefore Ferritic Steels) such as in Division 1 UCS,
and Ferritic Steels [highlight #FCE94F]With Properties Enhanced by Heat Treatment[/highlight] such as in Division 1 UHT. The other few references in Division 2 allow to make the same disctinction.

Now this makes sense, thank you again.



 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top