Hello!
I have a relatively simple engineering case that I hope you can help me with. I am trying to simulate the behavior of a flat "S shape" structure under deformation (50% strain). What I am expecting from designing such "S shape" structure is a release of strain by unfolding on the Z axis/normal plane, similar to this:
We made a little experiment using a thin 0.1mm Kapton tape to confirm this.
The results I am obtaining, however, do not match with the experimental results. The structure does not unfold on the Z axis (see results of U3 displacement below) and therefore there is a high concentration of stresses and strains (see results of S mises and E below).
I modeled this structure as a 3D deformable part with a shell section 0.1mm thick (overall structure is 16mm long), but it seems it is doing the simulation as if it was a 2D planar part. For the boundary conditions, the very left edge has the X displacement and Y=Z=0, and the right edge has X=Y=Z=0. I tried to change these boundary conditions slightly but results were the same.
I hope you can give me a little helping hand to solve the mistery. Thank you very much for your help, and happy holidays!
C.
----
- CAE file: - Undeformed shape: - Von Mises: - Strain: - Z displacement:
I have a relatively simple engineering case that I hope you can help me with. I am trying to simulate the behavior of a flat "S shape" structure under deformation (50% strain). What I am expecting from designing such "S shape" structure is a release of strain by unfolding on the Z axis/normal plane, similar to this:
We made a little experiment using a thin 0.1mm Kapton tape to confirm this.
The results I am obtaining, however, do not match with the experimental results. The structure does not unfold on the Z axis (see results of U3 displacement below) and therefore there is a high concentration of stresses and strains (see results of S mises and E below).
I modeled this structure as a 3D deformable part with a shell section 0.1mm thick (overall structure is 16mm long), but it seems it is doing the simulation as if it was a 2D planar part. For the boundary conditions, the very left edge has the X displacement and Y=Z=0, and the right edge has X=Y=Z=0. I tried to change these boundary conditions slightly but results were the same.
I hope you can give me a little helping hand to solve the mistery. Thank you very much for your help, and happy holidays!
C.
----
- CAE file: - Undeformed shape: - Von Mises: - Strain: - Z displacement: