Hello all,
I need a guidance.

I am working on a design for an ethanol 99.9% double skin tank to be located underground.
The tank should be made of stainless steel 304.
The tank shall be designed and constructed and tested according to some European code.
I usually design underground tanks according to EN-12285-1 but that code is for steel tanks and not stainless.

Can anyone please advise on what code i should be working with?

Detailing is a hobby,
 
Errr EN 12285-1.

Did you read it?


It's quite clear that the design includes stainless steels (section 6.2) including material code 1.4306 in appendix B to EN 10088-1, which appears to be the same as 304L.



Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
Dear Jay_ (Mechanical)

I have German version of the standart DIN EN-12285-1.

Annex B shows the applicable materials. I have copied and pasted below. AISI 304 L corresponding to Material 1.4306

Moreover, for ethanol, as per Line item 506 (page 67) Carbon Steel is permitted.


DIN_12285-1_ccjh6b.png
 
Hello,
thank you for your inputs,
I'm unfamiliar with the EN grade of stainless steel.