recomended or some code hydrotest pressure for gravity and pressure FRP piping

There is a 3500 m long pipe.Recomended length to be tested each time (1.5 m diameter ).To intall headers in each extreme of the pipe or a flange ?

Sorry so many questions

Regards ,


SPLIT
 
Replies continue below

Recommended for you

Normally if the pipes are supplied from Europe a 1.5 times the working pressure will be required to test the line. In the North american Market a 1.25 times is accepted.

If the pipeline is divided with valves, test between valves after installing test flanges to the the end flanges of the section.
 
steve,
I agree with you about the ISO-14692, but please check this standard and you will find that most GRE pipes produced in USA are not in accordance with the ISO requirments. Check the recommended GRE pipe produced in USA and europe about the recommended hydrotest pressure.
 
What difference does it make where the pipe is made? If ISO 14692 is the quoted specification the the supplier must comply with it.