First off, thanks for reading this! Here is my problem:
I am using dukane servo driven sonic welders to join together plastic cassette components. They are relatively decent sized, about 5 inches X 3 inches. They don't weld the entire surface, but only on the mating paths. My problem is that the bottom of the cassette gets all scuffed up during the process. I would like to make some sort of pad to put underneath the cassette that will prevent the plastic surface from being scuffed up yet also not interfere with the welding efficacy.
Does anyone have any sort of experience in the subject that may suggest a good material that won't deteriorate (quickly atleast) from the welding? My initial thought were just get something softer than the material being welded, but having no experience I wanted to ask here first.
thanks!
First off, thanks for reading this! Here is my problem:
I am using dukane servo driven sonic welders to join together plastic cassette components. They are relatively decent sized, about 5 inches X 3 inches. They don't weld the entire surface, but only on the mating paths. My problem is that the bottom of the cassette gets all scuffed up during the process. I would like to make some sort of pad to put underneath the cassette that will prevent the plastic surface from being scuffed up yet also not interfere with the welding efficacy.
Does anyone have any sort of experience in the subject that may suggest a good material that won't deteriorate (quickly atleast) from the welding? My initial thought were just get something softer than the material being welded, but having no experience I wanted to ask here first.
thanks!