May 27, 2020 #1 civst500 Structural Joined Nov 5, 2015 Messages 2 Location US I saw a now closed post that was asking the Ultimate strength of A615 and A706 rebar. A simple answer was not provided, as it should've been. A615 for Yield of 60 ksi, Ultimate = 90 ksi A706 Yield = 60 ksi, Ultimate = 80 ksi
I saw a now closed post that was asking the Ultimate strength of A615 and A706 rebar. A simple answer was not provided, as it should've been. A615 for Yield of 60 ksi, Ultimate = 90 ksi A706 Yield = 60 ksi, Ultimate = 80 ksi
May 27, 2020 #2 Guest090822 Structural Joined Jan 18, 2017 Messages 260 Location US civst500 - you will find there are no simple answers on this forum! One thing I’ve learned as am engineer is that we disagree more than we agree. Upvote 0 Downvote
civst500 - you will find there are no simple answers on this forum! One thing I’ve learned as am engineer is that we disagree more than we agree.