I saw a now closed post that was asking the Ultimate strength of A615 and A706 rebar. A simple answer was not provided, as it should've been.

A615 for Yield of 60 ksi, Ultimate = 90 ksi
A706 Yield = 60 ksi, Ultimate = 80 ksi
 
Replies continue below

Recommended for you

civst500 - you will find there are no simple answers on this forum! One thing I’ve learned as am engineer is that we disagree more than we agree.
 