Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Ultimate shear and ultimate tensile relation

Status
Not open for further replies.

fishercd

New member
Joined
Jun 5, 2002
Messages
5
Location
US
Is saying that the ultimate shear allowable is approx. equal to 0.6 times the ultimate tensile allowable if only the tensile allowable is known? I'm trying to "fix" a horribly made appendix and I've never encountered this relation before.
 
What material?
 
1/4-28 bolts. 80,000 psi tensile strength. that's all the information I have from the specs.
 
The Distortion-Energy theory states that the yield strength in shear is given by the equation;

Sxy=0.577 x Sy


The Maximum-Shear-Stress theory states that the yield strength in shear is given by the equation;

Sxy=0.50 x Sy

Ref Mechanical Engineering Design 4th ed Shigley pp 232, 234