UL94V-0 has to do with flammability. Basically it means that the stuff stops burning soon after you remove a flame from it, and doesn't emit flaming drips.
It's commonly specified for thermoplastics used as electrical insulation, and in any application where a material that makes a fire worse would be a bad thing.
Mike Halloran
Pembroke Pines, FL, USA