Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

UK Material BS3602/35

Status
Not open for further replies.

samuelliu

Mechanical
Joined
Jan 7, 2001
Messages
85
Location
CA
Does anyone know the spec (Chemical and mechanical properties)?
 
BS3602-1/360 equivalent to SA/A106 GR A, DIN 1626-st. 35.8, STPG370

TEN. 360~500 N/mm2
YIELD MIN. 215 "
ELONGATION MIN. 24%
C 0.17 MAX
Si 0.35 MAX
Mn 0.4~0.8
P 0.045 MAX
S 0.045 MAX



 
Hi, aobjr:

Thanks for your input, but BS3602 Grade 35 might be an out of dated standard, and I'm pretty sure that it is different with BS3602-1/360. Can you check it out again from your handbook?
 
I think your material specifiction is based on old standard.

Based on my data FROM LOWER GRADE TO HIGHER GRADE:

BS3601-360(SA/A53GRA,DIN 1626-st.35,STPG370)
BS3602-360(SA/A106GRA, DIN 17175-st.35.8,STPT370)
BS3602-410(SA/A106GRB, DIN 17175-st.45.8,STPT410)
BS3602-460(SA/A106GRC,STPT480)

HOPE ITS CLEAR TO YOU.
 