UG-99(g) exemption of gas leak test

Status
Not open for further replies.

cak4Engg

Petroleum
Joined
Jun 13, 2015
Messages
19
Location
AE



Query 1: In order to waive off the Visual inspection of welded joints as per UG-99(g),

[li]Does all the para of UG-99(g) (1), (2), (3) & (4) need to meet?[/li]
[li]Or meeting para of UG-99(g) (3), (4) waive Visual inspection of welded joints.[/li]

Query 2: Dose UG(99)(g)(2) can be substituted with 100% RT as per agreement with Inspector.
 
Provided there's not a Code Case on this:
Q1a: yes
Q1b: no
Q2: no
AFAIK, only CC2247 is on UG-99, but probably not for your application.
 