UCS SA-105 Clarification 1

Status
Not open for further replies.

ENG2194

Mechanical
Sep 12, 2019
45
In figure UCS-66 under the requirements of curve B, it says "A/SA-105 forged flanges produced to fine grain practice and normalized, normalized and tempered, or quenched and tempered after
forging

Is this read like: (produced to fine grain practice and normalized), (normalized and tempered), or (quenched and tempered)

or read that it must be produced to fine grain practice in addition to the following three options (normalized), (normalized and tempered), or (quenched and tempered)

???
 
Replies continue below

Recommended for you

As a note in the 2019 Edition it has been moved to Curve A
 
Oknow the quote i posted was from the 2019 edition. SA-105 as forged material has moved to curve A in the 2019 ed. A/SA-105 forged flanges, produced to fine grain practice and normalized, normalized and tempered, or quenched and tempered after forging, is on curve B.
 