hi

ucs-66(b)(3) describes if the material no need pwht but pwht done for it can reduction 17C ? or if pwht not requirement of this code (asme viii ) but the material required pwht by b31.3 (20mm) and this material repostweld can use 17c reduction ?
which ones are true?
 
Replies continue below

Recommended for you

Follow the Code you are using. You can't pick and choose parts from multiple codes. Where are you getting PWHT required for 20mm material in B31.3?
 