Dear experts,

For Loose-type flange (As per Fig. 3a of Appendix-2 - Thickness 101 mm) attached to Shell (Thickness - 12 mm), What shall be the governing thickness as per UCS-66??

Thanks in advance,



Thanks,

Rajput
 
RAJPT89, see UCS-66(a)(1)(-a)(-2). Thinner of the two parts joined.

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
Thanks Mike. I've already read that, but your reply boosted my confidence.

Thanks again.

Thanks,