Maximum rate of heating = 400 Deg.F
An item was PWHT to 800 deg. F then sat at 800F for 1 hr then increased to 1100F in a matter of 15 minutes, does this satisfy UCS-56(d), which states a maximum heating rate of 400F/hr above 800F?
Maximum rate of heating = 400 Deg.F