Hello, I am in section 9 of ASME and am trying to determine the types of testing that is required for a new weld procedure. Maybe I have over looked something, but to me it is not clear on the types of teating required. Can someone please get me going in the right direction. Thanks all
John
 
If it's a groove or fillet weld you want to qualify on review the Table QW 451.1.
 
I should clarify that fillets could be qualified without a groove weld. Look at QW 451.3 if that's a better fit for you.
 
Thanks so much. That is all I could find in code, but wanted some extra guidence. Thanks again
 