Dear All, --

I have a customer which want to coat their pipe of A.53 type, the thickness approximately 12.57 mm, what type of ceramic coatings should applied in this and how thick the coating to make their pipe resistant from heat and another substance.
thanks
 
What temperatures? What is "another" substance?

Why glass or ceramic coating? That is going to be very expensive and extremely difficult to install without damaging the liner which will make your corrosion issue worse.

I'd recommend a different metal or ptfe lined pipe.
 
is there a reson the customer wqants a ceramic coating?
 