I'm not happy with the anti-static spray cleaner that I'm using right now and I'm plannig to use 10% IPA wipes to clean bench tops, work stations and walls in my "Y" caoting room. Any suggestion? is this effective? are the wipes at 10% IPA regularated?

Tx.
 
What are you cleaning with the current cleaner? You can use 409 or fantastic instead of teh antti-static cleaner or use the anti-static cleaner after the 409 if cleanliness is your goal.
 