Working on a project in Wyoming. The contractor submitted a concrete mix with Type IP cement. The specs say Type II. Is there any issue with this? Concrete will be used for foundations only. Thanks for the input!
 
Replies continue below

Recommended for you

Double posting is discouraged.

thread507-500890
 