New at a job designing HDMI connectors. Still learning a bunch, appreciate it if anyone would care to explain a few terms on an engineering drawing I'm looking at:
Finish:
Ni UNDER PL
GOLD PL
TIN (MATTE)
[Matte is the question I have. Is it referring to it being the top layer of plating?]
Camber: 10 MAX/1000
Twist: 20° MAX/1000
FLEXED THE SIDE CUT FORM BY DIE DESIGN
It's a Japanese Engineering drawing
Thanks much
Casey