Does anyone know how to estimate the force that is put on an insert? I am working with some college students and they asked me for the force and I have never needed it and am not sure how to determine it.
 
Are you referring to "tool pressure"?
 
Yes. Tool pressure would be great.
 
If you can find a copy of 'Modern Metal Cutting' put out by Sandvik Coromant it covers the subject rather well.
 