Jul 29, 2010 #1 vinay0003 Chemical Joined Jul 29, 2010 Messages 6 Location IN i work for zinc smelter plant and we obtain sulphuric acid as by product and it is produced by contact process but the problem here is that the sulphuric acid that is being produced is turbid can anyone state the reasons for this
i work for zinc smelter plant and we obtain sulphuric acid as by product and it is produced by contact process but the problem here is that the sulphuric acid that is being produced is turbid can anyone state the reasons for this
Jul 30, 2010 #2 ash9144 Chemical Joined Jan 30, 2007 Messages 539 Location US Most likely iron sulfate from contact with carbon steel or cast iron or nitrates given off by the smelting process. Upvote 0 Downvote
Most likely iron sulfate from contact with carbon steel or cast iron or nitrates given off by the smelting process.