On a shell and tube heat exchanger and for tube-to-tubesheet welding.

QW-193 says nothing about the length of the tubes to be used for the mock-up itself. It also does not note the size of the mock tubesheet, only the thickness (2")
I'm using 10 x 10" and I'm hoping that is large enough.

Also, for these do you have to do a separate mocke for tubes that are welded vs tubes that are seamless?
 