Tube to tube sheet joint is expanded plus seal welded.
Is it better to expand the tube withing tube sheet prior to welding?
rather than expanding after welding?
Expansion prior to welding is an essential variable while qualifying the welding procedure, I have to make sure expansion before welding is preferable or after? so that same I can exercise at the time of qualification.
Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN
Is it better to expand the tube withing tube sheet prior to welding?
rather than expanding after welding?
Expansion prior to welding is an essential variable while qualifying the welding procedure, I have to make sure expansion before welding is preferable or after? so that same I can exercise at the time of qualification.
Nasir