We have a Low pressure steam boiler. It operates at around 45 kg/cm.2. Its a kettle type heat exchanger with straight tubes. Recently leakage was observed in the boiler.Inspection reavaled, that 06 tubes failed & many places tube to tube sheet weld leak was observed . The tubes are SA179 tubes. Steam is on shell side & tubes carrying the hot gases. It is importnat to note that All leaks were obserbed on the inlet side lower half (inlet tube sheet temp. is approx 570 Deg. C whereas outlet temp. is around 250 deg c). What could be the reason of this failure ? Inlet side shell support legs are fixed type where as outlet side shell support legs are floating. Upon inspection, it was observed that the tubes are bent along the length. This observation was made while peeping through the tubes.
Necessary repairs have been carried out.
WIll any one share his view about the problem & share the experience.
Necessary repairs have been carried out.
WIll any one share his view about the problem & share the experience.