Dear All,

We are manufacturing the shell & tube heat exchangers, and got additional testing requirement for client that is
" Tubes will have a control by current of Foucault according to the norm NF A49-872
(use Tube standard for Foucault current test n°100M4241")

Please suggest where I can found this standard, is this same as eddy current ?

Sorry if it has been discussed before.
 
Replies continue below

Recommended for you

Yes, the Foucault current or eddy current are the same think. Foucault has been credited with the discovery of eddy current.
 