We have to modify convection section in two fired heaters (oil refinery), to obtain a determined (by customer) outlet fuel gas temperature. So we have the following questions:
1. On their condictions, the shield section tube supports temperature design will be 2098°F; it is over API 560 indication (2000°F). What can we do? What material of tube supports is recomended on that temperature?
2. What can we do, if flue gas temperature gradient across a single convection intermediate tube support is over 400°F, indicated by API 560? In our case we have one case with 844°F and other case with 506°F.
Thanks,
1. On their condictions, the shield section tube supports temperature design will be 2098°F; it is over API 560 indication (2000°F). What can we do? What material of tube supports is recomended on that temperature?
2. What can we do, if flue gas temperature gradient across a single convection intermediate tube support is over 400°F, indicated by API 560? In our case we have one case with 844°F and other case with 506°F.
Thanks,