Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

True Stress/True Strain Data for Polymers

Status
Not open for further replies.

DRE111

Mechanical
Dec 20, 2004
10
I'm looking for true stress vs true strain into the plastic range for FEA modelling of PTFE, UHMWPE, Nylon, Delrin and other seal materials. Anybody have a good source?
 
Replies continue below

Recommended for you

Hi.

Performance of PTFE can be predicted by calculation similar to other engineering materials.

However, just as steel and aluminum properties are different, so, too, is PTFE from other engineering materials.

For tensile stress, stress-strain curves in the usual design temperatures show that yield occurs at high deformation. Elasticity begins to deviate from linearity at strains of only a few percent, like most plastics. Consequently, when working with PTFE or other plastic, it's best to work with acceptable strain and determine the corresponding stress.

For more information, just reference:

<a href=" Non Stick Coatings</a>

Consider, too, asking the major suppliers. For example, there's DuPont for PTFE, Arkema for nylon, Victrex for PEEK, etc.

Good luck!