Hi,

In my datasheet, it is written as "ASTM A-53, A-106, API-5L, GR B SMLS (TRIPLE RATED) for Pipe"..What is mean by Triple rated material..Is there any standard for it???

Thanks
 
I have a feeling it just means that the standards listed apply concurrently to apply the most restrictive specification envelop for the pipe.

Use translation assistance for Engineers forum

Note the rules include No Student posting
 
It meets the chemistry and testing requirements for all three materials specifications. Seamless carbon steel pipe is also often quadruple rated as SA/A-53B, SA/A-106B, API 5LB and API 5LX42.
 