Hi,

In my datasheet, it is written as "ASTM A-53, A-106, API-5L, GR B SMLS (TRIPLE RATED) for Pipe"..What is mean by Triple rated material..Is there any standard for it???

Thanks
 
Replies continue below

Recommended for you

It meets the chemistry and testing requirements for all three materials specifications. Seamless carbon steel pipe is also often quadruple rated as SA/A-53B, SA/A-106B, API 5LB and API 5LX42.
 