I have inquiry from my customer a relief valve for Vacuum Tower Bottoms Liquid service. He ask for Trim 5 material and that is not available at the moment. I would like to know whether other alternative material (e,g Stainless Steel 316) can take this service or not. Appreciate someone help me on that.
 
Replies continue below

Recommended for you

API Trim 5 is fully stellited (i.e., seat and disc) compared to, for example API trim 8 which is "half stellite", i.e., only the seat whereas the disc is 410. So you could move from API trim 8 to API trim 5 with confidence; however, shifting from API trim 5 to an SS316 trim means using API trim 10 (see the API trim chart: [URL unfurl="true"]http://alloy-valves.com/Alloy-Valves-Product-Range/API-600-trim-chart.php[/url]

Whether you can substitute API Trim 5 with API trim 10 depends on the process, and of course, on your customer's approval. Generally, however, there's a reason why valve trims are specified as they are; in case of a stellited specification, there may be concerns of with regard to corrosion, erosion, abrasion, sliding wear, oxidation, galling or pressure-temperature considerations.

Corrosion resistant, exotic alloy valves from The Alloy Valve Stockist in Barcelona, Spain [URL unfurl="true"]http://valvestockist.com[/url]
 