I am working on a custom residential project in Orange county, CA and wanted to know, if anyone has any experience using the Tridi (3-D) panels, as walls (and may be also as floor). These panels are manufactured in factory wtih 2-1/2" expanded polysterene (styroform) in the center and have 11GA steel bars at 6" o.c. in both directions, once these panels arrive on site, then the shotcrete is done on both sides, when they are standing in place. Any suggestions, info, would be helpful. I have gone through some material and ICBO report, I found. Thanks.
 